We recommend spraying the adhesion glue evenly on the glass before starting the print.
- Dirty glass will result in poor bed adhesion.
- An overly clean glass surface creates excessively strong adhesion, which may cause damage to the glass plate.
New 3D printers do not have such problems and can be ignored.
If there is no oil, heavy dust or glue residue on the surface of the build plate, please clean the plate with non-woven fabrics and pure alcohol.
New 3D printers do not have such problems and can be ignored.
Spray evenly on the build plate as what the video shows. ↑
Coat the right-nether corner of the build plate
Please remember to coat the glue on the red marked area, because the printhead will do pre-extrusion in this area.
If you want to fabricate channel letters using liquid acrylic craft, it means you will move the build plate into a curing machine without removing the 3D printed channel letters from the plate.
To make it easier to remove the letters after curing the liquid acrylic, we provide a dedicated glue for this craft.
Coat the glue evenly on the build plate. ↑
Coat the right-nether corner of the build plate
Please remember to coat the glue on the red marked area, because the printhead will do pre-extrusion in this area.